MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nylon

(Viewing data as-entered. Click here to return)
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Oilon was a break through of the first magnitude in the world of cast nylons, developed in the early 70s by Nylacast and introduced to the market in 1974. Oilon was the very first authentic lubricated Nylon, having a blended liquid lubricant system built in during the process stages, which obviously resulted in a substantial increase in bearing life, 5 times that of Natural cast nylon and 25 times that of phosphor bronze! The lubricant contained within the material will not drain, machine, spin, leech or dry out and never needs replenishment. A uniformed distribution of the lubricant throughout the product guarantees a constant performance over the whole service life and improvements in rate of wear, sliding frictional properties, abrasion resistance and stick slip performance are just a few of the benefits offered by this material. Oilon has been successful in considerably enlarging the application possibilities of nylons in many areas and specifically that of unlubricated moving parts. Oilon has acquired an unmatchable track record over the past 40 years and continues to go from strength to strength, for Nylacast has over this period produced thousands of tons of Oilon and the trend continues. There have been many imitators over the years since Oilon has been introduced, however, Oilon has not yet been equalled by its rivals and remains the premier oil-lubricated nylon available from any source. Oilon is suitable for use in applications in both the food and pharmaceutical industries.

Benefits:

  • First authentic lubricated nylon
  • Improved wear and abrasion resistance
  • Improved PV characteristics
  • Improved coefficient of friction and stick/slip characteristics
  • Consistent wear performance throughout product life
  • Reduced water absorption
  • Excellent mechanical, thermal and chemical resistance properties
  • Good dimensional stability
  • FDA compliant for direct food contact applications
  • Blended liquid lubricant system
Typical Application:
  • Wear pads
  • Support rails
  • Sheaves
  • Rollers
  • Guide plates
  • Bearings
  • Spacers
  • Pulleys
  • Spacers
  • Brake blocks
  • Conveyor rail
  • Pipe Clamps
  • Gears
  • Bushes
  • Wear Strips
  • Bespoke Components

Information provided by Nylacast Ltd.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.138 g/ccmethod A; ISO 1183:1987
Water Absorption 0.20 %
@Time 86400 sec
Immersion @ 23°C; ISO 62:1999
Moisture Absorption at Equilibrium 2.0 %50% RH, 23°C; ISO 62:1999
Water Absorption at Saturation 6.1 %
@Time 86400 sec
Immersion @ 23°C; ISO 62:1999
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ISO 868:2003
Tensile Strength, Yield 74.0 - 78.0 MPaSample Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break <= 30 %Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 3500 - 3700 MPaE-modulus; Type 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 105 - 125 MPa1.5mm/min; ISO 178:2001
Flexural Modulus 3300 - 3600 MPa1.5mm/min; ISO 178:2001
Compressive Strength 110 - 120 MPaType B, 5mm/min; ISO 604:2002
Compressive Modulus 2100 - 2600 MPaType B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 5.00 - 6.50 kJ/m²Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.089
@Pressure 1.75 MPa
31.4m/min
K Factor (Wear Factor) 2.2000
@Pressure 1.75 MPa
[m*3/Nm], 31.4m/min
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance >= 1.00e+14 ohmIEC 60093:1980-01
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 60250:1969-01
 4.0
@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mmIEC 60243-1:1998-01
Dissipation Factor 0.014
@Frequency 100 Hz
IEC 60250:1969-01
Comparative Tracking Index 600 VIEC 60112:2003-01
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-2:1999
Thermal Conductivity 0.250 W/m-KMean T = 20°C; ISO 8301:1991
Melting Point 221 °C
Maximum Service Temperature, Air 170 °CIntermittent
 110 °C
@Time 1.80e+7 sec
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75
Minimum Service Temperature, Air -100 °CIntermittent
 -40.0 °CContinuous
Glass Transition Temp, Tg 65.0 °CISO 11359:1999
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorGreen
Limiting PV100 MPa/m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nylacast Nylube Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant)
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled
Overview of materials for Nylon 6, MoS2 Filled
Akro-Plastic Akroloy® PA GF 30 natural (3177) PA 66 + PA 6I/6T Dry, 30% Glass Filled
Mitsubishi Chemical Advanced Materials Nylatron™ LIG Oil Filled Cast 6 Nylon

PNYLAC06 / 89264

Nylon

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.