MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Carbon/Epoxy Composite Rod
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Carbon Fiber - Epoxy Resin Matrix

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPaTransverse
 1100 - 1900 MPaLongitudinal
Elongation at Break 0.50 %Transverse - Tensile
 1.1 %Longitudinal - Tensile
Modulus of Elasticity 10.0 GPaTransverse
Tensile Modulus 120 - 140 GPaLongitudinal
Flexural Strength 1200 MPaLongitudinal
Flexural Modulus 125 GPaLongitudinal
Compressive Strain at Break 0.80 %Longitudinal
 2.5 %Transverse
Compressive Strength 50.0 - 250 MPaTransverse
 800 - 1300 MPaLongitudinal
 
Thermal PropertiesOriginal ValueComments
CTE, linear -0.700 - -0.300 µm/m-°C
@Temperature 20.0 °C
Longitudinal
CTE, linear, Transverse to Flow 28.0 µm/m-°C
@Temperature 20.0 °C
 
Descriptive Properties
Volume Fraction Fibers, %55-60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Carbon/Epoxy Composite Sheet
Aluminum 6151-T6
Goodfellow Carbon/Epoxy Composite Tube
Eagle Brass 210 Gilding Metal, Hard
DuPont Mobility and Materials Vespel® CP-9800 Carbon Fiber and Epoxy Composite, Ultra-high modulus end effectors

PGOODF119 / 42274

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.