MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboGlass-1 Epoxy Decoupage Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboGlass-1 is a combination of a clear resin compound and a clear hardener. It is a virtually colorless, clear liquid, 2-part, epoxy system for casting layers up to 2 or more inches, and for embedments. It is used on tabletops, counters, pictures, and artifacts. AboGlass-1 offers: (1) Virtually colorless, glass-like, transparency; (2) Low viscosity for pouring, wetting, and self-leveling; (3) superior hardness and abrasion resistance; (4) High impact resistance; (5) Outstanding water and weather resistance; (6) Machineable; (7) Superior tabletop resurfacer; (8) Can be applied in thick or thin layers. It offers the best recoat adhesion within the first 1-4 days. After this period, it should be sanded (or reprimed with the same Primkote 8006-1) if it is glossy and difficult to wet. It can also be used alone, in one or several coats, to protect metal surfaces from rust, to make a flat surface glossy, or to protect a color pattern.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
Density 8.80 lb/gal
Solids Content 100 %
Viscosity 1750 cP
 
Processing PropertiesOriginal ValueComments
Pot Life 25 min
 
Descriptive Properties
GlossHigh
Hardening Time (min)40-50
Induction Period (min)5 to 10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Atom Adhesives AA-BOND F110 Epoxy Adhesive
Overview of materials for Epoxy Adhesive
Overview of materials for Epoxy Cure Resin
Aremco Aremco-Bondâ„¢ 2330 High Performance Epoxide
Arlon Electronic Materials 45N Multifunctional Epoxy Laminate and Prepreg

PABC842 / 107826

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.