MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite SUMILITE® ELC-4972R&S Glass Epoxy Laminate
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Glass Epoxy Double sided Materials for PCB

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.090 %E-24/50+D-24/23
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 12.0 GPaTD
 14.0 GPaMD
Flexural Strength 300 MPaTD
 350 MPaMD
Flexural Modulus 16.0 GPaTD
 18.0 GPaMD
Peel Strength 1.40 kN/mA; 18umCF
 1.40 kN/mS-20"/260; 18umCF
Film Tensile Strength at Break, MD 160 MPa
Film Tensile Strength at Break, TD 100 MPa
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.1
@Frequency 1e+9 Hz
C-96/20/65
 4.2
@Frequency 1e+9 Hz
C-96/20/65+D-24/23
 4.5
@Frequency 1e+6 Hz
C-96/20/65
 4.5
@Frequency 1e+6 Hz
C-96/20/65+D-24/23
Dissipation Factor 0.018
@Frequency 1e+9 Hz
C-96/20/65
 0.019
@Frequency 1e+9 Hz
C-96/20/65+D-24/23
 0.020
@Frequency 1e+6 Hz
C-96/20/65
 0.022
@Frequency 1e+6 Hz
C-96/20/65+D-24/23
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 47.0 µin/in-°F10°C/min; Z (a1)
 300 µin/in-°F10°C/min; Z (a2)
CTE, linear, Transverse to Flow 20.0 µin/in-°F10°C/min; X (a1)
 24.0 µin/in-°F10°C/min; Y (a1)
Glass Transition Temp, Tg 110 °C20°C/min
 125 °C10°C/min
 150 °C5°C/min
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fibre Glast Epolite 2427 Epoxy
Fibre Glast EZ Poxy EZ10 / EZ83 Epoxy
Fibre Glast ProSet 125R / 229H Epoxy
Fibre Glast RAE 2426 / 2177 Epoxy
Solvay CYCOM® 5216 Epoxy - Unidirectional S-Glass Prepreg

PSUMIT117 / 193922

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.