System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 30% Glass Fiber Filled
Material Notes:
Ultramid B3ZG6 BK30564 is an impact-modified, pigmented black, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.33
g/cc
0.0480
lb/in³
ISO 1183
Water Absorption
5.9 - 6.5 %
5.9 - 6.5 %
ISO 62
Moisture Absorption at Equilibrium
1.8 - 2.2 %
1.8 - 2.2 %
23°C/50% R.H.; ISO 62
Viscosity Measurement
160
160
Viscosity Number; ISO 307
Linear Mold Shrinkage
0.0050
cm/cm
0.0050
in/in
Melt Flow
33.25
g/10 min
@Load 5.00 kg,
Temperature 275 °C
33.25
g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
150
MPa
21800
psi
50mm/min; ISO 527
Elongation at Yield
3.6 %
3.6 %
50mm/min; ISO 527
Modulus of Elasticity
9.00
GPa
1310
ksi
ISO 527
Flexural Strength
220
MPa
31900
psi
ISO 178
Flexural Modulus
7.40
GPa
1070
ksi
ISO 178
Izod Impact, Notched (ISO)
20.0
kJ/m²
9.52
ft-lb/in²
ISO 180/A
10.0
kJ/m²
@Temperature -30.0 °C
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
Charpy Impact Unnotched
2.00
J/cm²
@Temperature -30.0 °C
9.52
ft-lb/in²
@Temperature -22.0 °F
ISO 178
Charpy Impact, Notched
2.00
J/cm²
9.52
ft-lb/in²
ISO 179/1eU
9.50
J/cm²
45.2
ft-lb/in²
ISO 179/1eA
3.50
J/cm²
@Temperature -30.0 °C
16.7
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+13
ohm-cm
1.00e+13
ohm-cm
IEC 60093
Dielectric Constant
3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor
0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
550
V
550
V
Test Solution A; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
20.0
-
25.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
11.1
-
13.9
µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow
60.0
-
70.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
33.3
-
38.9
µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Thermal Conductivity
0.350
W/m-K
2.43
BTU-in/hr-ft²-°F
DIN 52612
Melting Point
220
°C
428
°F
DIN 53765
Maximum Service Temperature, Air
180
°C
356
°F
Deflection Temperature at 0.46 MPa (66 psi)
220
°C
428
°F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
200
°C
392
°F
ISO 75
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Processing Properties
Metric
English
Comments
Melt Temperature
270
-
290
°C
518
-
554
°F
Injection-molding/Extrusion
Mold Temperature
80.0
-
90.0
°C
176
-
194
°F
Injection-molding
Descriptive Properties
Color
BK30564
Commercial Status
North America and Europe
Impact Modified
Yes
Primary Processing Technique
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
EMS-Grivory Grilon® BGZ-30/2 PA6-GF30
BASF Ultramid® B3ZG6 BK 30564 30% Glass Filled PA6-1 (Conditioned)
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry)
EMS-Grivory Grilon® BGZ-30 PA6-GF30
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry)
PBASF9346 / 85110
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.