MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company VLF 80211 EM HS Nylon 6/6 (PA), Long Glass Fiber - Easy Molding - Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 60% Glass Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.71 g/ccASTM D 792
Additive Loading 60 %Primary Additive
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.17 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40000 psiASTM D 638
Elongation at Break 1.5 - 2.5 %ASTM D 638
Tensile Modulus 3250 ksiASTM D 638
Flexural Strength 60000 psiASTM D 790
Flexural Modulus 2900 ksiASTM D 790
Izod Impact, Notched 10.0 ft-lb/in
@Thickness 3.17 mm
ASTM D 256
Izod Impact, Unnotched 30.0 ft-lb/in
@Thickness 3.17 mm
ASTM D 4812
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 480 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 470 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 520 - 570 °F
Mold Temperature 150 - 255 °F
Drying Temperature 175 °F
@Time 7200 - 14400 sec
Moisture Content 0.20 %
Dew Point 0.000 °F
Injection Pressure 5000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1045 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round
Chase Plastics CP Pryme® NN130M2HS (Dry) Nylon 66, 30% Glass Fiber Reinforced, Lubricated, Heat Stabilized
Overview of materials for Nylon 66, 60% Glass Fiber Filled
RTP Company RTP 285 G FR HS Nylon 4/6 (PA), Carbon Fiber - Flame Retardant - Heat Stabilized - Dry As Molded
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Conditioned, 60% Glass Filled

PQZTA1013 / 159085

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.