MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 2061-22 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Overview: CALIBRE™ 2061-22 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-22 provides exceptional clarity, heat resistance, impact strength, and processability, and has low contamination levels. CALIBRE 2061-22 resin has undergone biocompatibility testing based on ISO 10993 (Biological Evaluation of Medical Devices) and is suitable for use in approved medical applications. This product contains mold release.

Main Characteristics:

  • ISO 10993
Applications:
  • Medical applications

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183/A; ASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62; ASTM D570
Moisture Absorption at Equilibrium 0.32 %
@Temperature 23.0 °C
50% RH; ISO 62; ASTM D570
Melt Flow 22 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 65.5 MPa50 mm/min; ASTM D638
 66.0 MPaISO 527-2/50
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527-2/50; ASTM D638
Elongation at Break 120 %50 mm/min; ISO 527-2/50; ASTM D638
Tensile Modulus 2340 MPa50 mm/min; ISO 527-2/50; ASTM D638
Flexural Strength 96.5 MPaMethod I (3 point load), 2.0 mm/min; ISO 178; ASTM D790
Flexural Modulus 2410 MPaMethod I (3 point load), 2.0 mm/min; ISO 178; ASTM D790
Izod Impact, Notched 750 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Notched (ISO) 73.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Dart Drop, Total Energy 72.3 J3.39 m/sec; ASTM D3763
Abrasion 45[%] Taber; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+17 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
 17.0 kV/mmIEC 60243-1
Dissipation Factor 0.0010
@Frequency 50 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 142 °CAnnealed; ISO 75-2/B; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °CUnannealed; ASTM D648; ISO 75-2/A
 126 °CAnnealed; ASTM D648; ISO 75-2/A
Vicat Softening Point 152 °C
@Load 5.10 kg
Rate A (50°C/h); ISO 306/B50; ASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542; ISO 489
Haze 1.0 %ASTM D1003
Transmission, Visible 89 %ASTM D1003
 
Descriptive Properties
Average Extent of Burring3 cmASTM D635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 2061-15 Polycarbonate Resin
Dow Tyril® 100 SAN
Trinseo CALIBRE™ 2061-6 Polycarbonate Resin
Trinseo CALIBRE™ 5051 15 Polycarbonate, 5% Glass Reinforced
Trinseo TYRIL™ 875 SAN Resin

PDWST028 / 142237

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.