MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 1581 Polyester, Briquette, Transfer Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and flammability ratings. UL recognized under component file E40654. 01581 is available in a wide range of colors.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.810 g/cc0.0293 lb/in³ASTM D1895
Density 1.83 g/cc0.0661 lb/in³ASTM D792
Water Absorption 0.099 %0.099 %ASTM D570
Linear Mold Shrinkage 0.00179 cm/cm0.00179 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 6666ASTM D785
Tensile Strength, Ultimate 77.0 MPa11200 psiASTM D638
Elongation at Break 0.94 %0.94 %ASTM D638
Tensile Modulus 12.9 GPa1870 ksiASTM D638
Flexural Strength 119 MPa17300 psiASTM D790
Flexural Modulus 10.6 GPa1540 ksiASTM D790
Compressive Strength 178 MPa25800 psiASTM D695
Poissons Ratio 0.310.31ASTM D638
Shear Modulus 4.92 GPa714 ksiCalculated
Izod Impact, Notched 0.560 J/cm1.05 ft-lb/inASTM D256
Charpy Impact, Notched 0.610 J/cm²2.90 ft-lb/in²ASTM D256
Impact 294294J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.10e+15 ohm-cm1.10e+15 ohm-cmASTM D247
Dielectric Constant 4.44.4ASTM D150
Dielectric Strength 11.6 kV/mm295 kV/inStep by Step; ASTM D149
 14.4 kV/mm366 kV/inShort Time; ASTM D149
Dielectric Breakdown 22900 V22900 V1hr 120C; ASTM D149
Dissipation Factor 0.01720.0172ASTM D150
Arc Resistance 189 sec189 secASTM D495
Comparative Tracking Index 600 V600 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C
@Temperature 40.0 - 130 °C
35.0 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 209 °C408 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 278 °C532 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.00 mm
V-0
@Thickness 0.0394 in
Oxygen Index 46 %46 %ASTM D2863
Shrinkage 0.0259 %0.0259 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 1501 Polyester, Briquette, Transfer Molded
Plenco 1500 Polyester, Granular, Transfer Molded
Plenco 1500 Polyester, Granular, Compression Molded
Plenco 1510 Polyester, Granular, Transfer Molded
Plenco 1508 Polyester, Briquette, Transfer Molded

PLEL26 / 50594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.