MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plenco 1581 Polyester, Briquette, Transfer Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and flammability ratings. UL recognized under component file E40654. 01581 is available in a wide range of colors.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.810 g/ccASTM D1895
Density 1.83 g/ccASTM D792
Water Absorption 0.099 %ASTM D570
Linear Mold Shrinkage 0.00179 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 66ASTM D785
Tensile Strength, Ultimate 77.0 MPaASTM D638
Elongation at Break 0.94 %ASTM D638
Tensile Modulus 12.9 GPaASTM D638
Flexural Strength 119 MPaASTM D790
Flexural Modulus 10.6 GPaASTM D790
Compressive Strength 178 MPaASTM D695
Poissons Ratio 0.31ASTM D638
Shear Modulus 4.92 GPaCalculated
Izod Impact, Notched 56.0 J/mASTM D256
Charpy Impact, Notched 0.610 J/cm²ASTM D256
Impact 294J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.10e+15 ohm-cmASTM D247
Dielectric Constant 4.4ASTM D150
Dielectric Strength 11.6 kV/mmStep by Step; ASTM D149
 14.4 kV/mmShort Time; ASTM D149
Dielectric Breakdown 22900 V1hr 120C; ASTM D149
Dissipation Factor 0.0172ASTM D150
Arc Resistance 189 secASTM D495
Comparative Tracking Index 600 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 63.0 µm/m-°C
@Temperature 40.0 - 130 °C
TMA; ASTM E831
Maximum Service Temperature, Air 209 °CHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 278 °CASTM D648
Flammability, UL94 V-0
@Thickness 1.00 mm
Oxygen Index 46 %ASTM D2863
Shrinkage 0.0259 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plenco 1501 Polyester, Briquette, Transfer Molded
Plenco 1500 Polyester, Granular, Transfer Molded
Plenco 1500 Polyester, Granular, Compression Molded
Plenco 1510 Polyester, Granular, Transfer Molded
Plenco 1508 Polyester, Briquette, Transfer Molded

PLEL26 / 50594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.