MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® H24 Electrically Conductive Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Product Description: EPO-TEK® H24 is a two component, electrically and thermally conductive epoxy adhesive designed for semiconductor die attach and hybrid micro-electronics assembly.

Advantages & Application Notes:

  • Low density silver-filled epoxy is ideal for ultrasound and acoustical applications of electronics.
  • Extended pot-life allows for mass production and low waste.
  • Suggested Applications:
    • Hybrid Micro-electronics: SMD and die attach on Au pads and ceramic substrates. Single step curing method of die and SMDs.
    • Electronics: compatible with piezo technologies for ultrasound circuits found in medical, industrial, and petrochemical industries.
    • Scientific / Life Sciences: geo-thermal, geo-seismic, infra-sound, as well as acoustical-optical circuits for interferometers and lasers.
    • Optical: bright and shiny silver flake is advantageous for LED die-attach.
  • A smooth and creamy paste allows for automated or hand dispensing, pin transfer, or screen printing application methods of manufacture.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccPart B
 2.10 g/ccPart A
Particle Size <= 45 µm
Viscosity 15000 - 23000 cP
@Temperature 23.0 °C
10 rpm
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) 88 ppm
Ionic Impurities - K (Potassium) 8.0 ppm
Ionic Impurities - Cl (Chloride) 60 ppm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76
Tensile Modulus 485000 psiStorage
Shear Strength >= 1700 psiDie
 >= 2000 psiLap
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.020 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.0 µm/m-°CBelow Tg
 104 µm/m-°CAbove Tg
Thermal Conductivity 0.670 W/m-K
Maximum Service Temperature, Air 250 °CContinuous
 350 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 100 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Decomposition Temperature 470 °CDegradation Temperature
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 150 °C
Minimum Bond Line
 10.0 min
@Temperature 120 °C
Minimum Bond Line
 20.0 min
@Temperature 100 °C
Minimum Bond Line
 45.0 min
@Temperature 80.0 °C
Minimum Bond Line
Pot Life 1080 min
Shelf Life 6.00 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorAmberPart B
 SilverPart A
ConsistencySmooth paste
Ionic Impurities NH421 ppm
Mix Ratio by Weight100:5
Number of ComponentsTwo
Thixotropic Index1.86
Weight Loss0.04%200°C
 0.04%250°C
 0.1%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 310M-2 Optically Clear, Flexible Epoxy
Epoxy Technology EPO-TEK® H20E-8 Electrically Conductive, Silver Epoxy
Epoxy Technology EPO-TEK® H20E-175 Electrically Conductive, Silver Epoxy

PPOXYT039 / 141078

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.