MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bales Mold Service Dia-Clust® (Diamond-Chrome) Mold Coating
Categories: Metal; Metal Matrix Composite; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Description: Dia-Clust®, also known as Diamond-Chrome, is a chromium matrix composite coating with an ultra-high dispersion of nanometer-sized, spherical -shaped diamond particles that give mold protection of at least 25% better than hard chrome plating alone. It is applied at very low temperatures to any metal without compromising its shape or size, it can be applied at any thickness and is very strippable.

Applications: Moving components slides, rotating cores, locks, etc.

Information provided by Bales Mold Service.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C >= 85
Coefficient of Friction <= 0.15
 
Processing PropertiesOriginal ValueComments
Processing Temperature 130 °FApplied Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Diamond, Polycrystalline
Diamond, thin film
IBC Advanced Alloys Beralcast® 191 Beryllium-Aluminum Alloy
Iron Silicide, FeSi2
MarkeTech Silicon Single Crystal Semiconductor Wafer, p-type, Boron Doped, Czochralski-LED Grown

NBAL0 / 15079

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.