MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ed Fagan EFI Alloy 50 Soft Magnetic Alloy
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: Features high initial permeability, maximum permeability, and low core loss.

Key Words: ASTM A753, MIL N-14411
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.295 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 80
Tensile Strength, Ultimate 518 MPa
Tensile Strength, Yield 159 MPa
Elongation at Break 40 %in 2"
Modulus of Elasticity 166 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000490 ohm-cm
Magnetic Permeability 100000Typical DC
Magnetic Coercive Force, Hc 0.060 OeTypical DC
Magnetic Saturation Flux Density, Bmax 14500 GaussTypical DC
Curie Temperature 450 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µin/in-°F
@Temperature 25.0 - 450 °C
Specific Heat Capacity 0.120 BTU/lb-°F
Thermal Conductivity 90.0 BTU-in/hr-ft²-°F
Melting Point 1427 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Iron, Fe <= 49 %
Manganese, Mn <= 0.50 %
Nickel, Ni 50 %
Silicon, Si <= 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ed Fagan EFI Alloy 79 Soft Magnetic Alloy
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled
FloMet Fe-3% Si Soft Magnetic Alloy
FloMet Permalloy® 4-79 Moly Soft Magnetic Alloy
Overview of materials for T 400 Series Stainless Steel

NEDFA9950 / 194940

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.