MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PSI 4440(AS) High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: 4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, the flow properties of this grade make it particularly suitable for the molding of large parts and for use with new techniques such as gas injection.

Applications: Television front and back covers, Office equipment

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines. This product was previously known as LACQRENE®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D1505
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238G
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 76ASTM D785
Tensile Strength, Yield 250 kg(f)/cm²ASTM D638M
Elongation at Break 55 %ASTM D638M
Flexural Yield Strength 40.0 kg(f)/cm²ASTM D790
Flexural Modulus 20000 kg(f)/cm²ASTM D790
Izod Impact, Notched 10.0 kg-cm/cmASTM D256A
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+13 ohmISO IEC93
Dielectric Strength 150 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 91.0 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °CASTM D648
Vicat Softening Point 88.0 °C50N; ASTM D1525B
 96.0 °C10N; ASTM D1525A
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 240 °C
Drying Temperature 70.0 °CPre drying temperature
Dry Time 2 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PSC 1540(AS) Crystal Polystyrene
Total Lacqrene® 4241 High Impact Polystyrene
Total Lacqrene® 3351(AS) Impact Polystyrene
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin
Ineos Nova S-5400 High Impact Compact Polystyrene

PFINAA040 / 38476

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.