MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 9370A Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion- and injection molding grade; very good hydrolysis and microbial resistance; good low-temperature flexibility; free from plasticizers; high moisture vapor transmission rate; Application; breathable films; Seals, membranes; Films; hard - soft systems; Sports shoe soles.

Mechanical property data for samples at 50% RH.

Information provided by Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70
@Time 1.00 sec
70
@Time 0.000278 hour
DIN ISO 7619-1
Tensile Strength, Ultimate 25.7 MPa3730 psi200mm/min; DIN 53504
Elongation at Break 738 %738 %200mm/min; DIN 53504
Tensile Modulus  0.00900 GPa
@Temperature 60.0 °C
1.31 ksi
@Temperature 140 °F
Tensile Storage Modulus; ISO 6721-1,-4
 0.0110 GPa
@Temperature 20.0 °C
1.60 ksi
@Temperature 68.0 °F
Tensile Storage Modulus; ISO 6721-1,-4
 0.125 GPa
@Temperature -20.0 °C
18.1 ksi
@Temperature -4.00 °F
Tensile Storage Modulus; ISO 6721-1,-4
100% Modulus 3.50 MPa
@Strain 100 %
508 psi
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus 6.70 MPa
@Strain 200 %
972 psi
@Strain 200 %
200 mm/min; DIN 53504
Rebound 63 %63 %ISO 4662
Tear Strength 39.0 kN/m223 pli500mm/min; ISO 34-1
Abrasion 6969mm3; ISO 4649 method A, 50% RH
Compression Set  22 %
@Temperature 72.0 °C,
Time 82800 sec
22 %
@Temperature 162 °F,
Time 23.0 hour
DIN ISO 815-1
 35 %
@Temperature 70.0 °C,
Time 86400 sec
35 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1, Method C
 51 %
@Temperature 70.0 °C,
Time 86400 sec
51 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1, Method A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 175 - 210 °C347 - 410 °Fextrusion
 190 - 210 °C374 - 410 °Finjection molding
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °Finjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 9370AU Polyurethane
Covestro Desmopan® 9380A Thermoplastic Polyurethane
Covestro Desmopan® 3070AU Thermoplastic Polyurethane
Covestro Desmopan® 89043D Thermoplastic Polyurethane
Covestro Desmopan® 385 E Polyurethane

PB095014 / 200085

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.