MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay Thornel® Mat VMA Carbon Fiber  (discontinued **)
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Composed of high strength, high modulus carbon filaments in a random-layered orientation. The fine diameter filaments are up to three inches long and are mechanically bonded to form a continuous web of materials ~1 inch thick, 20.5 inches wide that is supplied in rolls 60-80 feet long.

98% carbon assay, 13 µm filament diameter

Solvay has acquired the Thornel product line as a part of the Cytec purchase.

Key Words: Carbon Fibre
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/ccFilament Property.
Apparent Bulk Density 0.0360 g/cc
Specific Surface Area 0.40 m²/gFilament Property
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1400 MPaFilament Property. Mat strength is 120 N/m
Tensile Modulus 170 GPaFilament property
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00120 ohm-cmFilament
 0.700 ohm-cmMat
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.410 W/m-Kacross thickness of mat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)
Solvay Thornel® VCB-20 Carbon Fiber Cloth
Solvay Thornel® Graphite Cloth
Solvay Thornel® Mat VMC Carbon Fiber
Solvay Thornel® Mat VME Carbon Fiber

ETHORM / 6094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.