MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type S21904 (Alloy 21-6-9) Stainless Steel, cold rolled sheet, 25% cold reduction
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: Austenitic, high strength, excellent corrosion resistance, and low magnetic permeability. Applications include aircraft applications such as ducting and bellows systems, tail pipes and exhaust systems, clamps, fasteners, flanges, and hydraulic tubing.

Key Words: UNS S21904, AMS 5595, AMS 5656, ASME SA412, ASTM A269 (XM-11), ASTM A276 (XM-11), ASTM A314 (XM-11), ASTM A412 (XM-11), ASTM A473 (XM-11), ASTM A580 (XM-11)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.83 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 326Converted from Rockwell C hardness.
Hardness, Knoop 352Converted from Rockwell C hardness.
Hardness, Rockwell C 35
Hardness, Vickers 340Converted from Rockwell C hardness.
Tensile Strength, Ultimate 1097 MPa
 592 MPa
@Temperature 650 °C
 715 MPa
@Temperature 540 °C
 798 MPa
@Temperature 425 °C
 877 MPa
@Temperature 315 °C
 931 MPa
@Temperature 205 °C
 998 MPa
@Temperature 95.0 °C
Tensile Strength, Yield 876 MPa
@Strain 0.2 %
 500 MPa
@Strain 0.2 %,
Temperature 650 °C
 601 MPa
@Strain 0.2 %,
Temperature 540 °C
 667 MPa
@Strain 0.2 %,
Temperature 425 °C
 759 MPa
@Strain 0.2 %,
Temperature 315 °C
 836 MPa
@Strain 0.2 %,
Temperature 205 °C
 881 MPa
@Strain 0.2 %,
Temperature 95.0 °C
Elongation at Break 14.5 %in 50 mm
 5.5 %
@Temperature 205 °C
in 50 mm
 6.0 %
@Temperature 315 °C
in 50 mm
 8.0 %
@Temperature 650 °C
in 50 mm
 9.0 %
@Temperature 540 °C
in 50 mm
 10.5 %
@Temperature 425 °C
in 50 mm
 12 %
@Temperature 95.0 °C
in 50 mm
Modulus of Elasticity 200 GPaTypical for stainless steel
Machinability 30 %Based on 100% machinability for AISI 1212 steel.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000730 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.7 µm/m-°C
@Temperature 25.0 - 95.0 °C
 17.3 µm/m-°C
@Temperature 25.0 - 205 °C
Annealed
 18.2 µm/m-°C
@Temperature 25.0 - 315 °C
Annealed
 19.1 µm/m-°C
@Temperature 25.0 - 540 °C
 20.0 µm/m-°C
@Temperature 25.0 - 760 °C
Annealed
 20.0 µm/m-°C
@Temperature 25.0 - 870 °C
Annealed
 20.5 µm/m-°C
@Temperature 25.0 - 980 °C
Annealed
Specific Heat Capacity 0.480 J/g-°CTypical value for stainless steel.
Thermal Conductivity 7.80 W/m-K
@Temperature -180 °C
 10.9 W/m-K
@Temperature -73.0 °C
 13.8 W/m-K
@Temperature 95.0 °C
 16.1 W/m-K
@Temperature 205 °C
 18.2 W/m-K
@Temperature 315 °C
 20.2 W/m-K
@Temperature 425 °C
 22.5 W/m-K
@Temperature 540 °C
 24.7 W/m-K
@Temperature 650 °C
 26.8 W/m-K
@Temperature 760 °C
 28.9 W/m-K
@Temperature 870 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.040 %
Chromium, Cr 20 %
Iron, Fe 64 %
Manganese, Mn 9.0 %
Nickel, Ni 6.0 %
Nitrogen, N 0.23 %
Phosphorus, P <= 0.060 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 651 (19-9) Stainless Steel cold rolled and stress relieved, 35 HRC hardness
ASTM A606 HSLA Steel, Cold Rolled Sheet
AISI 1022 Steel, cold rolled, 25 mm (1 in.) round
AISI 1018 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI Type S21900 (21-6-9) Stainless Steel, cold rolled sheet, 25% cold reduction

MQM22FE / 13755

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.