MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® P1011 Electrically Conductive Modified Polyimide
Categories: Polymer; Adhesive; Thermoset; Polyimide, TS

Material Notes: Product Description: EPO-TEK® P-1011 is a single component, modified polyimide, silver-filled adhesive designed for chip bonding in microelectronic and optoelectronic applications.

Advantages & Application Notes:

  • Low stress die-attach adhesive that is very effective for bonding quartz crystal oscillators used in Rf / Microwave wireless devices.
  • Designed specifically for screen printing and machine dispensing applications. A lower viscosity version, called P1011S is available for die-stamping processes.
  • Recommended for screen printing applications; long dry time.
  • Good electrical and thermal conductivity.
  • Suggested for ceramic and DIP packaging of hybrids, as well as TO-Cans.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.39 g/cc
Particle Size <= 20 µm
Viscosity 8000 - 12000 cP
@Temperature 23.0 °C
20 rpm
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) 39 ppm
Ionic Impurities - K (Potassium) 18 ppm
Ionic Impurities - Cl (Chloride) 114 ppm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61
Shear Strength >= 1700 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.00050 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.0 µm/m-°CBelow Tg
 225 µm/m-°CAbove Tg
Thermal Conductivity >= 2.74 W/m-K
Maximum Service Temperature, Air 225 °CContinuous
 325 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 100 °CRamp 40°C/Min to 300°C
Decomposition Temperature 389 °CDegradation Temperature
 
Processing PropertiesOriginal ValueComments
Dry Time <= 168 hour
Cure Time 30.0 min
@Temperature 80.0 °C
Pre-Bake, Minimum Bond Line
 90.0 min
@Temperature 285 °C
Post-Cure, Minimum Bond Line
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorSilver
ConsistencySmooth slightly thixotropic paste
Ionic Impurities NH427 ppm
Number of ComponentsSingle
Thixotropic Index1.9
Weight Loss0.06%200°C
 0.08%250°C
 0.15%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Atom Adhesives AA-DUCT 905 Epoxy Adhesive
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer
Atom Adhesives AA-BOND F253 Epoxy Adhesive
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy
NuSil EPM-2463 Silicone, Thermal Interface Material (TIM): Electrically Conductive

PPOXYT051 / 141090

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.