MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Medical Grade Stainless Steel 316LVM
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: This ‘Medical Grade’ stainless steel 316 is vacuum melted to achieve the extremely high levels of purity and ‘cleanliness’ required for surgical implants. Also used for high precision electronic parts. It has excellent resistance in physiological environments, to general and intergranular corrosion, to pitting and crevice corrosion.

Stress relieve at 250°C for one hour then air cool after final forming.

Information provided by Alloywire International and Sandvik.

Key Words: W.NR 1.4441; UNS S31673; AWS 163. Meets standards BS 7252 Pt1 COMPOSITION D; ASTM F138
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 160Annealed Bar
 300High Tensile Bar
Tensile Strength at Break 490 - 800 MPaAnnealed
 1100 MPaHigh Tensile Bar
 1300 - 2200 MPaSpring Temper Wire
Tensile Strength, Yield 190 MPa
@Strain 0.2 %
Annealed Bar
 800 MPa
@Strain 0.2 %
High Tensile Bar
Elongation at Break 12 %High Tensile Bar
 45 %Annealed Bar
Modulus of Elasticity 187.5 GPa
Poissons Ratio 0.33Calculated
Shear Modulus 70.3 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.485 J/g-°C
Thermal Conductivity 14.0 W/m-K
Melting Point 1500 °C
Maximum Service Temperature, Air 300 °Cannealed or spring temper wire
Minimum Service Temperature, Air -200 °Cannealed or spring temper wire
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 17 - 19 %
Iron, Fe 60.5 - 67.75 %as balance
Manganese, Mn <= 2.0 %
Molybdenum, Mo 2.25 - 3.5 %
Nickel, Ni 13 - 15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Bioline 316LVM Bar Steel
AISI Type 316L Stainless Steel, annealed and cold drawn bar
316 Stainless Steel, annealed bar
Titanium Ti-6Al-4V (Grade 5), Annealed
Sandvik Bioline 316LVM Tube and pipe, seamless

MQ316Rm / 88080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.