MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey Active-braze™ No. 10 Brazing Paste Grade B420P 75
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Active-braze™ No.10 Brazing Paste Grade B402P 75 is a specialized brazing paste for the active brazing of non-metallic materials. Employing an active brazing technique removes the need for prior metallization of the non-metallic material such as the “molymanganese” metallization commonly applied to alumina ceramics.

Active-braze™ No.10 brazing paste is formulated around a silver, copper filler metal with an addition of titanium as the active element. The paste binder system used in the product is a water soluble polymer type.

Active type brazing filler metals do not flow by capillary or spread significantly like most brazing filler metals and need to be placed within the joint. Active-braze™ No.10 has a brazing temperature range of 780 to 950°C

Active-braze™ No.10 is used for the brazing of ceramics like alumina and zirconia, diamond, natural, single crystal or CVD (chemical vapor deposition) types, as well as graphite, sapphire, silicon carbide and PCBN (polycrystalline cubic boron nitride) to themselves or to metallic substrates like low expansion nickel alloys, copper and tungsten carbide.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 780 - 800 °C
Solidus 780 °C
Liquidus 800 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 28 %
Silver, Ag 70 %
Titanium, Ti 2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Boron Nitride, Cubic BN, (Borazone)
Momentive Performance Materials AC6041 Boron Nitride (BN) Powder
Silicon Carbide, Alpha SiC
Diamond, Natural
Diamond, Polycrystalline

NJMMJ9898 / 186299

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.