MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Supreme Petrochem SP 253 Toughened Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Characteristics
  • High rigidity
  • Improved toughness
  • Good clarity
Processing
  • Injection molding
Applications
  • Ball pens
  • Small appliances housings
  • Small impellers
Material Status: Commercial : Active

Agency Ratings: FDA 21 CFR 177.1640

Information provided by Supreme Petrochem LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 42.2 MPa50 mm/min; ASTM D638
Elongation at Break 5.0 %50 mm/min; ASTM D638
Flexural Strength 58.8 MPa
@Thickness 3.20 mm
ASTM D790
Flexural Modulus 22000 kg(f)/cm²
@Thickness 3.20 mm
ASTM D790
Izod Impact, Notched 15.0 J/m
@Thickness 3.20 mm
ASTM D256
Izod Impact, Unnotched 2.00 J/cm
@Thickness 3.20 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °CASTM D648
Vicat Softening Point 103 °C1kg load; 120°C/h; ASTM D1525
Flammability, UL94 HB
@Thickness 1.60 mm
 
Optical PropertiesOriginal ValueComments
Haze 2.5 %
@Thickness 1.00 mm
Transmission, Visible 88 %
@Thickness 1.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature <= 220 °C
Mold Temperature 40.0 - 50.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chesterton ARC 982 100% Novolac acid resistant coating
Chesterton ARC 855 Abrasion Control Coating
Vyncolit X655 Novolac Phenolic
Vyncolit X6151 Novolac Phenolic
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation

PSUP27 / 69459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.