MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 10.9 ksi
@Temperature 93.3 °C
90°, Dry
 11.7 ksi
@Temperature 25.0 °C
90°, Dry
 63.5 ksi
@Temperature 25.0 °C
Open Hole Tensile, Dry
 107 ksi
@Temperature 25.0 °C
Quasi-Isotropic 25/50/25, Dry
 276 ksi
@Temperature -55.0 °C
0°, Dry
 293 ksi
@Temperature 90.6 °C
0°, Dry
 310 ksi
@Temperature 25.0 °C
0°, Dry
Tensile Modulus 1220 ksi
@Temperature 200 °C
90°, Dry
 1390 ksi
@Temperature 77.0 °C
90°, Dry
 19100 ksi
@Temperature 195 °C
0°, Dry
 19400 ksi
@Temperature -67.0 °C
0°, Dry
 19600 ksi
@Temperature 77.0 °C
0°, Dry
Flexural Yield Strength 274 ksi
@Temperature 25.0 °C
0°, Dry
Flexural Modulus 18400 ksi
@Temperature 25.0 °C
0°, Dry
Compressive Yield Strength 27.0 ksi
@Temperature 25.0 °C
After 2500 in-in-lb/in impact, Dry
 28.0 ksi
@Temperature 25.0 °C
After 2000 in-in-lb/in impact, Dry
 32.0 ksi
@Temperature 25.0 °C
After 1500 in-in-lb/in impact, Dry
 34.6 ksi
@Temperature 25.0 °C
Compression After Impact, Dry
 50.0 ksi
@Temperature 25.0 °C
After 500 in-in-lb/in impact, Dry
 91.2 ksi
@Temperature 25.0 °C
Compression Before Impact, Dry
 184 ksi
@Temperature 90.6 °C
0°, Dry
 184 ksi
@Temperature 90.6 °C
0°, Wet
 203 ksi
@Temperature 71.1 °C
0°, Wet
 222 ksi
@Temperature 25.0 °C
0°, Dry
 230 ksi
@Temperature -55.0 °C
0°, Dry
Compressive Modulus 17000 ksi
@Temperature 71.1 °C
0°, Wet
 17700 ksi
@Temperature 90.6 °C
0°, Dry
 18000 ksi
@Temperature -55.0 °C
0°, Dry
 18100 ksi
@Temperature 90.6 °C
0°, Wet
 18600 ksi
@Temperature 25.0 °C
0°, Dry
Shear Strength 11.3 ksi
@Temperature 90.6 °C
0° Short Beam, Wet
 12.2 ksi
@Temperature 71.1 °C
0° Short Beam, Wet
 14.7 ksi
@Temperature 90.6 °C
0° Short Beam, Dry
 15.2 ksi
@Temperature 93.3 °C
+/- 45° In-Plane, Dry
 16.6 ksi
@Temperature 25.0 °C
+/- 45° In-Plane, Dry
 16.9 ksi
@Temperature 25.0 °C
0° Short Beam, Wet
 18.5 ksi
@Temperature 25.0 °C
0° Short Beam, Dry
 23.8 ksi
@Temperature -55.0 °C
0° Short Beam, Dry
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °FEpoxy Matrix Limit

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® 8552 Epoxy Matrix
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Hexcel® HexTow® IM7 6K Intermediate Modulus Carbon Fiber (6000 Filaments)
Hexcel® HexTow® IM7 Carbon Fiber - Epoxy Composite
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber

PHEXC052 / 98522

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.