System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
BASF Ultraform® N2640 Z2 POM + PUR
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Homopolymer, Unreinforced, Impact Grade
Material Notes:
Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.
Information provided by BASF
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Bulk Density
0.650
-
0.850
g/cc
Density
1.37
g/cc
ISO 1183
Water Absorption
0.80 %
ISO 62
Moisture Absorption at Equilibrium
0.20 %
ISO 62
Linear Mold Shrinkage, Flow
0.019
cm/cm
ISO 2577
Linear Mold Shrinkage, Transverse
0.019
cm/cm
ISO 2577
Melt Flow
9.59
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
110
MPa
@Load 36.5 kg,
Time 30.0 sec
ISO 2039-1
Tensile Strength, Yield
50.0
MPa
50 mm/min; ISO 527-1/-2
Elongation at Break
45 %
50 mm/min, Nominal; ISO 527-1/-2
Elongation at Yield
12 %
50 mm/min; ISO 527-1/-2
Tensile Modulus
2000
MPa
ISO 527-1/-2
Charpy Impact Unnotched
230
kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched
6.50
kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
11.0
kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+12
ohm-cm
IEC 60093
Surface Resistance
1.00e+14
ohm
IEC 60093
Dielectric Constant
4.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor
0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
600
V
Test Solution A; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
130
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point
167
°C
ISO 11357-1/-3
Maximum Service Temperature, Air
100
°C
Deflection Temperature at 1.8 MPa (264 psi)
85.0
°C
ISO 75-1/-2
Decomposition Temperature
>=
240
°C
Flammability, UL94
HB
@Thickness 1.60 mm
Ignition Temperature
320
-
340
°C
ASTM D1929
Processing Properties
Original Value
Comments
Processing Temperature
200
°C
Hopper Throat
Zone 1
200
°C
Feed zone
Zone 2
200
°C
Compression
Zone 3
200
°C
Metering-zone
Zone 4
200
°C
Nozzle
Melt Temperature
200
°C
Optimal
190
-
215
°C
Injection molding
Mold Temperature
60.0
°C
Optimal
60.0
-
80.0
°C
Injection molding
Drying Temperature
100
°C
Dry Time
3
hour
Descriptive Properties
Color
Black
Commercial Status
Europe
Peripheral Screw Speed
<0.3 m/s
Primary Processing Technique
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Avient Gravi-Tech™ GRV-UR-110-W Polyurethane, PUR
Evonik VESTAGON® B 1065 PUR System
Aluminum 5154-H112
BASF Ultraform® N2644 Z9 POM + PUR
Covestro Baydur® GS PUR Polyurethane
PBASG0163 / 131796
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.