MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMODUR® LU-T70D + BAYTEC® XL 1705 Polyurethane, TDI-PTMEG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccDESMODUR® LU-T70D
 1.21 g/ccBAYTEC® XL 1705
Viscosity 690 cPBAYTEC® XL 1705
 850 cPDESMODUR® LU-T70D
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70DIN 53505
 62
@Temperature 80.0 °C
DIN 53505
 73
@Temperature -5.00 °C
DIN 53505
Tensile Strength at Break 52.0 MPaDIN 53504
Tensile Stress at Strain 27.4 MPa
@Strain 10 %
DIN 53504
Elongation at Break 274 %DIN 53504
100% Modulus 0.0357 GPa
@Strain 100 %
DIN 53504
200% Modulus 0.0431 GPa
@Strain 200 %
DIN 53504
Resilience 40[%]; DIN 53512
Tear Strength 656 pliwith nick; ISO 34-1
 999 pliwithout nick; ISO 34-1
Compression Set 80 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815-1
 
Processing PropertiesOriginal ValueComments
Processing Temperature 30.0 °CBAYTEC® XL 1705
 60.0 °CDESMODUR® LU-T70D
Mold Temperature 100 °C
Pot Life 1.583 min
 
Descriptive Properties
AppearanceliquidDESMODUR® LU-T70D
 liquidBAYTEC® XL 1705
Content100Parts by weight of prepolymer
 20.6Parts by weight of BAYTEC® XL 1705
 8.3-8.7%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMODUR® LU-D80 + MOCA Polyurethane, TDI-Ester
Covestro DESMODUR® LU-T80 + BAYTEC® XL 1705 Polyurethane, TDI-PTMEG
Covestro DESMODUR® LU-T60D + BAYTEC® XL 1705 Polyurethane, TDI-PTMEG
Covestro DESMODUR® LU-T75D + BAYTEC® XL 1705 Polyurethane, TDI-PTMEG
Covestro DESMODUR® LU-T80 + BAYTEC® XL 2190 Polyurethane, TDI-PTMEG

PCOVEST0376 / 202159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.