MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
329 Stainless Steel, annealed bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: diameter of 25-75 mm

Key Words: UNS S32900, ASME SA268, ASTM A268, ASTM A511, SS 14 2324, SIS 14 2324, 453S, ASTM A 240, A240
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 230
Hardness, Knoop 253Converted from Brinell
Hardness, Rockwell B 96
Hardness, Rockwell C 28Alternate Reference
Hardness, Vickers 242Converted from Brinell
Tensile Strength, Ultimate 620 MPaAlternate Reference
 725 MPa
Tensile Strength, Yield 485 MPaAlternate Reference
 550 MPa
@Strain 0.2 %
Elongation at Break 15 %Alternate Reference
 25 %in 50 mm
Charpy Impact 54.0 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000750 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.4 µm/m-°C
@Temperature 20.0 - 815 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
Melting Point 1450 - 1510 °C
Solidus 1450 °C
Liquidus 1510 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.10 %
Chromium, Cr 28 %
Iron, Fe 63 %
Manganese, Mn <= 2.0 %
Molybdenum, Mo 1.5 %
Nickel, Ni 4.5 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
329 Stainless Steel, annealed strip
329 Stainless Steel, annealed tube
329 Stainless Steel, annealed pipe
AISI Type 651 (19-9 DL) Stainless Steel
Bisalloy Steels BisPlate 320 Thickness 5 -<16 mm

MQ329B / 12821

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.