MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmodur® E 23 A Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Desmodur E 23 A is an aromatic polyisocyanate prepolymer based on diphenylmethane diisocyanate (MDI). It is suitable as a binder for the formulation of moisture-curing, one-component coatings and adhesives. It is also suitable as a hardener for hydroxyl-bearing co-reactants.

Properties / Applications: Desmodur E 23 A is suitable for use in the formulation of moisture-curing one-component systems which, when thinned with a suitable solvent, can be used as primers and sealers for porous substrates to provide protection against moisture, oil, fuel and other chemicals. It can also be used as a binder in the formulation of synthetic resin mortars. Coatings formulated with Desmodur E 23 A are used as highgrade anti-corrosion systems for steel in civil and hydraulic engineering applications. In combination with suitable Desmophen polyols, Desmodur E 23 A yields tough but flexible, wear-resistant coatings and sealers. Desmodur E 23 A is also suitable for use in the formulation of solvent-free moisture-curing one-component adhesives or in combination with Baycoll to formulate two-component adhesives. These can be used to bond many materials, e.g. wood, metal and plastic. As with any product, use of Desmodur E 23 A in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/cc
Viscosity 1550 - 2050 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 193 °C
 
Descriptive Properties
Content15-15.8%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmodur® E 21 Polyurethane
Covestro Desmodur® H Polyurethane
Covestro Desmodur® E 744 Polyurethane
Covestro Desmodur® E 28 Polyurethane
Covestro Desmodur® E 2200/76 Polyurethane

PCOVEST0338 / 202121

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.