MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® B 30 GF NT AL Nylon PA6-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Vydyne B 30 GF NT AL is standard flow, 30% glass-fiber reinforced PA6 resin suitable for food contact applications. Available in natural, this product is also lubricated for improved machine feed and flow.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccDAM; ISO 1183
Water Absorption 1.1 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 2.1 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 180 MPaDAM; ISO 527-2
Elongation at Break 3.0 %DAM; ISO 527-2
Tensile Modulus 9500 MPaDAM; ISO 527-2
Flexural Strength 260 MPaDAM; ISO 178
Flexural Modulus 8200 MPaDAM; ISO 178
Poissons Ratio 0.34ISO 527-2
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Charpy Impact Unnotched 65.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 75.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 85.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 25.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
Comparative Tracking Index 600 V
@Thickness 3.00 mm
IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 220 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 210 °CUnannealed; DAM; ISO 75-2/A
Flame Spread 102 mm/min
@Thickness 2.00 mm
ISO 3795
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 260 °CInjection
Mold Temperature 80.0 - 90.0 °CInjection
Drying Temperature 80.0 - 90.0 °CInjection
Dry Time >= 3.00 hourInjection
 
Descriptive Properties
AdditiveLubricant
AppearanceNatural Color
FeaturesChemical Resistant
 Gasoline Resistant
 General Purpose
 Good Flow
 Good Heat Resistance
 Lubricated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8818 / 293387

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.