MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Rilsan® Clear G350 Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Rilsan® Clear G350 is a high performance transparent polyamide. This grade has been specially designed for injection molding applications, ideally suited for optics as high end eyewear frames.

Information provided by Arkema Group

Property data for dry samples, unless noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/ccISO 1183
Water Absorption 3.0 %Sim. to ISO 62
Moisture Absorption 1.10 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cmISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4 2577
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
MVR (cm³/10min); ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78
@Time 15.0 sec
ISO 868
Tensile Strength, Yield 51.0 MPaConditioned; ISO 527-1/-2
Elongation at Break >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 8.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 1480 MPaConditioned; ISO 527-1/-2
Flexural Modulus 1.34 GPaconditioned 15 days, 23°C - 50 % R.H.; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75-1/-2
Glass Transition Temp, Tg 145 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 V-2
@Thickness 3.20 mm
IEC 60695-11-10
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 92 %ISO 13468-1 -2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 10724
 
Descriptive Properties
FormPellets
Processing MethodsInjection Molding
 Other Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsan® Clear G170 Polyamide
Arkema Rilsan® Clear G300 HI PA
Arkema Rilsan® Clear G120 Rnew® PA
Arkema Rilsan® Clear G850 Rnew® PA
EPICHEM PA 6 Polyamide 6

PZARKG652_b / 149071

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.