MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 52G1 V20 GREY R7035 PA 6 20% Glass Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Description: TECHNYL C 52G1 V20 GREY R7035 is a 20% glass fiber reinforced, halogen and red phosphorus free flame retarded grade based on polyamide 6, for injection molding. This product is available in grey color.

Key Properties: GWFI 960°C; Excellent electrical performance; Easy processing; Good surface aspect

Benefits: This grade is Halogen and Red Phosphorous free fire resistant flame retardant grade with excellent molding and electrical performance.

Applications: It is particularly suitable for equipment requiring robust glow-wire resistance such as for MCB housings, contactors and switches and sockets.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183/A
Water Absorption 1.1 %
@Time 86400 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 65.0 MPaISO 527 Type 1A
Tensile Modulus 4550 MPaISO 527 Type 1A
Charpy Impact Unnotched 79.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 3.40 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 8.60 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 27.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CISO 11357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 70K20HSL BK284 PA66-RF20
Domo TECHNYL® C 52G1 V20 GREY R7035 PA 6 20% Glass Reinforced, Dry
Amco PRIMATOP PP HOMO 040 Polypropylene for Cast Film
Domo TECHNYL® C 246SI V11 PA6, 11% glass filled, DRY
Domo TECHNYL® C 218 V50 BLACK PA 6 50% Glass Reinforced, Conditioned

PSOLVAY866 / 218594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.