MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tellurium, Te
Categories: Metal; Nonferrous Metal; Other Engineering Material; Semiconductor; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.23 g/cc
a Lattice Constant 4.45 Å
c Lattice Constant 5.91 Å
Vapor Pressure 0.001013 bar
@Temperature 505 °C
 0.01013 bar
@Temperature 617 °C
 0.1013 bar
@Temperature 768 °C
 1.013 bar
@Temperature 988 °C
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 127.601995
Atomic Number 52
Thermal Neutron Cross Section 4.7 barns/atom
X-ray Absorption Edge 0.38972 ÅK
 2.50272 ÅLI
 2.68253 ÅLII
 2.85162 ÅLIII
Electronegativity 2.1Pauling
Ionic Radius 0.560 ÅCrystal Ionic Radius for Valence +6
 0.700 ÅCrystal Ionic Radius for Valence +4
 0.820 ÅCrystal Ionic Radius for Valence +1
 2.11 ÅCrystal Ionic Radius for Valence -2
 2.50 ÅCrystal Ionic Radius for Valence -1
Electrochemical Equivalent 0.99 g/A/h
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 25
Tensile Strength, Ultimate 11.0 MPa
Modulus of Elasticity 40.0 GPa
Poissons Ratio 0.33
Shear Modulus 15.16 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000150 ohm-cm
Magnetic Susceptibility -0.0000395Atomic (cgs)
 -3.10e-7cgs/g
Critical Superconducting Temperature 2.40 - 5.10 K
@Pressure 3800 - 5500 MPa
Te II
 4.10 - 4.50 K
@Pressure 5300 - 6200 MPa
Te III
 >= 4.72 K
@Pressure 6300 - 8000 MPa
Te IV
Band Gap 0.33 eV
Electron Mobility, cm²/V-s 1700
Hole Mobility, cm²/V-s 1200
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 30.6 J/g
Heat of Vaporization 666 J/g
CTE, linear 16.8 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.1965 J/g-°C
Thermal Conductivity 1.97 W/m-KPerpendicular to c-axis
 3.38 W/m-KParallel to c-axis
Melting Point 449.5 °C
Boiling Point 988 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 3.30
 
Component Elements PropertiesOriginal ValueComments
Tellurium, Te 100 %
 
Descriptive Properties
CAS Number13494-80-9

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Selenium, Se
Silicon, Si
Tin, Sn
Silver, Ag
Terbium, Tb

AMETe00 / 113

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.