MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Styrenic Elastomer (TES)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.400 - 11.0 g/ccAverage value: 1.04 g/cc Grade Count:1465
Water Absorption 0.0500 %Average value: 0.0500 % Grade Count:8
Viscosity 0.600 - 30000 cPAverage value: 3630 cP Grade Count:37
 1600 - 2300 cP
@Temperature 180 - 180 °C
Average value: 2080 cP Grade Count:4
Viscosity Measure 0.900 - 1800 cStAverage value: 64.7 cSt Grade Count:41
Linear Mold Shrinkage 0.000 - 0.0470 cm/cmAverage value: 0.0150 cm/cm Grade Count:345
Linear Mold Shrinkage, Transverse 0.00100 - 0.0190 cm/cmAverage value: 0.00861 cm/cm Grade Count:23
Melt Flow 0.100 - 220 g/10 minAverage value: 24.9 g/10 min Grade Count:274
Spiral Flow 23.0 - 85.0 cmAverage value: 53.4 cm Grade Count:42
 15.0 - 120 cm
@Temperature 200 - 200 °C
Average value: 72.8 cm Grade Count:70
 15.0 - 120 cm
@Pressure 76.0 - 76.0 MPa
Average value: 72.8 cm Grade Count:70
Ash 0.0100 - 39.0 %Average value: 4.60 % Grade Count:44
 
Chemical PropertiesOriginal ValueComments
Butadiene Content 60.0 - 78.0 %Average value: 70.1 % Grade Count:11
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 2.00 - 97.0Average value: 59.6 Grade Count:1393
Hardness, Shore D 23.0 - 74.0Average value: 38.8 Grade Count:107
Hardness, Shore C 9.00 - 23.0Average value: 15.7 Grade Count:3
Hardness, Shore OO 32.0 - 70.0Average value: 47.6 Grade Count:5
Tensile Strength, Ultimate 0.138 - 80.0 MPaAverage value: 7.87 MPa Grade Count:1373
Tensile Strength, Yield 0.586 - 26.0 MPaAverage value: 4.35 MPa Grade Count:23
Film Elongation at Break, MD 100 - 850 %Average value: 526 % Grade Count:35
Film Elongation at Break, TD 100 - 1100 %Average value: 601 % Grade Count:15
Elongation at Break 3.50 - 1900 %Average value: 604 % Grade Count:1425
Modulus of Elasticity 0.00105 - 54.0 GPaAverage value: 4.07 GPa Grade Count:22
Flexural Yield Strength 2.66 - 24.1 MPaAverage value: 15.4 MPa Grade Count:5
Flexural Modulus 0.0000910 - 2.02 GPaAverage value: 0.389 GPa Grade Count:30
Rebound 22.0 - 65.0 %Average value: 46.9 % Grade Count:27
Flex Crack Resistance 35000 - 132000Average value: 79700 Grade Count:5
Adhesive Bond Strength 0.550 - 2.65 MPaAverage value: 1.13 MPa Grade Count:10
Izod Impact, Notched 0.641 - 5340 J/cmAverage value: 2.02 J/cm Grade Count:14
Izod Impact, Unnotched 1.60 - 5340 J/cmAverage value: 2.14 J/cm Grade Count:10
Coefficient of Friction 0.720 - 3.42Average value: 1.81 Grade Count:9
Penetration 50.0Average value: 50.0 Grade Count:4
Penetration P(0), 1/10 mm 50.0 - 60.0Average value: 54.5 Grade Count:6
Tear Strength 2.94 - 113 kN/mAverage value: 27.4 kN/m Grade Count:1040
 45.0 - 163 kN/m
@Temperature -30.0 - 80.0 °C
Average value: 102 kN/m Grade Count:2
Peel Strength 1.75 - 6.14 kN/mAverage value: 4.73 kN/m Grade Count:14
Compression Set 5.00 - 99.0 %Average value: 40.7 % Grade Count:739
Tensile Set 90.0 - 95.0 %Average value: 91.7 % Grade Count:6
 33.0 - 95.0 %
@Temperature 70.0 - 70.0 °C
Average value: 58.4 % Grade Count:15
 33.0 - 95.0 %
@Time 79200 - 79200 sec
Average value: 58.4 % Grade Count:15
Film Tensile Strength at Break, MD 2.00 - 21.0 MPaAverage value: 7.55 MPa Grade Count:35
Film Tensile Strength at Break, TD 4.00 - 9.00 MPaAverage value: 6.23 MPa Grade Count:12
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0100 - 1.00e+16 ohm-cmAverage value: 1.76e+15 ohm-cm Grade Count:62
Surface Resistance 0.200 - 9.90e+12 ohmAverage value: 3.39e+11 ohm Grade Count:16
Static Decay 2.00 secAverage value: 2.00 sec Grade Count:5
Dielectric Constant 2.30 - 2.41Average value: 2.37 Grade Count:3
Dielectric Strength 24.0 - 39.4 kV/mmAverage value: 26.9 kV/mm Grade Count:37
Dissipation Factor 0.00300 - 0.00400Average value: 0.00343 Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.20 - 1.30 µm/m-°CAverage value: 1.25 µm/m-°C Grade Count:4
CTE, linear, Transverse to Flow 2.70 µm/m-°CAverage value: 2.70 µm/m-°C Grade Count:4
Melting Point 104 - 249 °CAverage value: 172 °C Grade Count:4
Maximum Service Temperature, Air 55.0 - 170 °CAverage value: 106 °C Grade Count:119
Heat Distortion Temperature 70.0 - 100 °CAverage value: 76.1 °C Grade Count:44
Minimum Service Temperature, Air -60.0 - -30.0 °CAverage value: -52.8 °C Grade Count:155
Brittleness Temperature -70.0 - -21.0 °CAverage value: -59.1 °C Grade Count:94
Glass Transition Temp, Tg -89.0 - -59.0 °CAverage value: -71.3 °C Grade Count:3
Flammability, UL94 HB - V-0Grade Count:70
Flame Spread 37.0 - 68.0 mm/minAverage value: 46.6 mm/min Grade Count:16
Oxygen Index 26.0 - 31.0 %Average value: 27.7 % Grade Count:9
Ring & Ball Softening Point 78.0 - 135 °CAverage value: 102 °C Grade Count:10
 
Optical PropertiesOriginal ValueComments
Haze 3.70 - 35.0 %Average value: 12.5 % Grade Count:18
Transmission, Visible 90.0 %Average value: 90.0 % Grade Count:29
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 221 °CAverage value: 163 °C Grade Count:110
Nozzle Temperature 171 - 280 °CAverage value: 196 °C Grade Count:251
Adapter Temperature 179 - 249 °CAverage value: 202 °C Grade Count:52
Die Temperature 174 - 249 °CAverage value: 198 °C Grade Count:82
Melt Temperature 149 - 280 °CAverage value: 188 °C Grade Count:436
Mold Temperature 10.0 - 80.0 °CAverage value: 34.6 °C Grade Count:315
Injection Velocity 13.0 - 25.0 mm/secAverage value: 19.0 mm/sec Grade Count:43
Drying Temperature 50.0 - 100 °CAverage value: 71.5 °C Grade Count:326
Moisture Content 0.0300 - 0.500 %Average value: 0.0783 % Grade Count:60
Dew Point -17.8 °CAverage value: -17.8 °C Grade Count:5
Injection Pressure 1.38 - 124 MPaAverage value: 40.9 MPa Grade Count:149
Cushion 0.381 - 2.54 cmAverage value: 0.949 cm Grade Count:57

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
Overview of materials for Polyester Thermoplastic Elastomer
Overview of materials for Polyether Block Amide (PEBA)
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade

O4990 / 78451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.