MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SPHERE ONE EXTENDOSPHERES™ 350 Hollow Spheres
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: EXTENDOSPHERES™ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheres™ replace heavier, more expensive components on an equivalent volume basis, they can reduce raw material costs as well as density.

Applications: EXTENDOSPHERES™ 350 hollow spheres are a standard grade. They are recommended for use in cement, grout, sealants, roofing compounds, PVC and latex flooring. They can also be used in high mil-build industrial coatings and mastics.

Information provided by Sphere One Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 g/cc
Density 0.700 - 0.800 g/cc
Particle Size 150 µmAverage Mean
 10 - 500 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 5.0
Compressive Strength 3000 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1300 °CDeformation temp
 
Component Elements PropertiesOriginal ValueComments
Al2O3 28 - 33 %
Fe2O3 <= 4.0 %
SiO2 58 - 65 %
 
Descriptive Properties
Colorgray
Physical FormFree-Flowing Powder
Shell ThicknessApprox. 10% of diameter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Syntac® 350 Composite Materials Syntactic Foam
Trelleborg AEM Syntac® Eccolite® Ultra
Trelleborg Emerson & Cuming Eccolite® Composite Materials Ultra Syntactic Foam
Trelleborg AEM Syntac® 350 Syntactic Foam
Thermal Ceramics Cerafiber® Bulk Fiber

CSPHERE01 / 2197

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.