MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® B3 GF 30 1 black (2485) Nylon 6, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Reinforced. Standard. PA 6 GF 30

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Filler Content 30 %ISO 1172
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPa5 mm/min. Conditioned; ISO 527-2
 185 MPa5 mm/min. Dry as Molded; ISO 527-2
Elongation at Break 3.0 %5 mm/min. Dry as Molded; ISO 527-2
 5.5 %5 mm/min. Conditioned; ISO 527-2
Tensile Modulus 6200 MPa1 mm/min. Conditioned; ISO 527-2
 10300 MPa1 mm/min. Dry as Molded.; ISO 527-2
Flexural Strength 270 MPaDry as Molded. 2 mm/min; ISO 178
Flexural Modulus 8500 MPa2 mm/min. Dry as Molded; ISO 178
Charpy Impact Unnotched 85.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179-1/1eA
 85.0 kJ/m²
@Temperature -30.0 °C
Dry as Molded; ISO 179-1/1eA
 95.0 kJ/m²
@Temperature 23.0 °C
Dry as Molded; ISO 179-1/1eA
 105 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179-1/1eA
Charpy Impact, Notched 12.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179-1/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Dry as Molded; ISO 179-1/1eA
 13.0 kJ/m²
@Temperature 23.0 °C
Dry as Molded; ISO 179-1/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+10 ohmConditioned; IEC 60093
 1.00e+12 ohmDry as Molded; IEC 60093
Comparative Tracking Index 600 VConditioned. Test solution A; IEC 60112
 600 VDry as Molded. Test solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDry as Molded. DES, 10°C/min; DIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 220 °CDry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 210 °CDry as Molded; ISO 75
Deflection Temperature at 8.0 MPa 150 °CDry as Molded; ISO 75
Flammability, UL94 HB
@Thickness 1.60 mm
Conditioned
 HB
@Thickness 1.60 mm
Dry as Molded
Glow Wire Flammability Index 650 °CConditioned; IEC 60695-2-12
 650 °CDry as Molded; IEC 60695-2-12
 
Descriptive Properties
Burning Rate<100 mm/minDry as Molded. FMVSS 302. >1 mm thickness
 <100 mm/minConditioned. FMVSS 302. >1 mm thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKRO9829 / 255486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.