MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties remain constant after moisture absorption up to a temperature of 60°C [140°F], for instance, for automotive valve housings.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.800 g/cc0.0181 - 0.0289 lb/in³
Density 1.43 g/cc0.0517 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.80 - 1.2 %0.80 - 1.2 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 4.3 - 5.3 %4.3 - 5.3 %ISO 62
Viscosity Measurement 130130ISO 307
Linear Mold Shrinkage 0.0035 cm/cm0.0035 in/inrestricted
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 2577
 0.0033 cm/cm0.0033 in/inTM=320°C, TW=100°C
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 210 MPa30500 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 3.0 %3.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 12.0 GPa1740 ksiISO 527-1/-2
Charpy Impact Unnotched 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.70 J/cm²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Dielectric Constant 4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 - 60.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
27.8 - 33.3 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
CTE, linear, Transverse to Flow 15.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
8.33 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°FDIN 52612
Melting Point 295 °C563 °FDIN 53765
Maximum Service Temperature, Air 135 °C275 °Ffor 50% loss of tensile strength after 20000hr
 160 °C320 °Ffor 50% loss of tensile strength after 5000hr
 270 °C518 °F
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FISO 75-1/-2
Decomposition Temperature >= 350 °C>= 662 °F
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Ignition Temperature >= 470 °C>= 878 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 300 °C572 °FFeed Zone
Zone 2 310 °C590 °FCompression
Zone 3 320 °C608 °FMetering-zone
Zone 4 320 °C608 °FNozzle
Melt Temperature 310 - 330 °C590 - 626 °FInjection-molding/Extrusion
 320 °C608 °FOptimal
Mold Temperature 80.0 - 120 °C176 - 248 °FInjection-molding
 100 °C212 °FOptimal
Drying Temperature 110 °C230 °F
Dry Time 8 hour8 hour
Moisture Content <= 0.030 %<= 0.030 %Optimal
 <= 0.15 %<= 0.15 %
 
Descriptive Properties
ColorBK 00564
Commercial StatusEurope
Peripheral Screw Speed<0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry)
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned)
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Conditioned)
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)

PBASG0292 / 131925

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.