MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese FORTRON 203 PPS, Unfilled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: A very easy flowing unfilled grade. This grade demonstrates excellent chemical resistance and thermal stability. Intended for extrusion applications that do not require high melt strength and for compounding with various fillers. Available as Fortron 0203B6 (granular powder), 0203P6 (pellets), and 0203C6 (crystallized pellets).

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Density 1.35 g/ccISO 1183
Water Absorption 0.010 %
@Temperature 22.8 °C
24hr immersion; ASTM D570
Water Absorption at Saturation 0.020 %ISO 62
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 93ASTM D785
 100ISO 2039-2
Tensile Strength at Break 33.0 MPa5mm/min; ISO 527-2/1A
 12500 psiASTM D638
Elongation at Break 1.0 %5mm/min; ISO 527-2/1A
 3.0 %ASTM D638
Tensile Modulus 4200 MPa50mm/min; ISO 527-2/1A
Flexural Strength 135 MPaISO 178
 21000 psiASTM D790
Flexural Modulus 3900 MPaISO 178
 600000 psiASTM D790
Izod Impact, Notched 0.500 ft-lb/inASTM D256
Izod Impact, Unnotched 11.0 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 2.00 kJ/m²ISO 180/1A
 8.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmIEC 60093
 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 1000 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
 4.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 17.0 kV/mmIEC 60243-1
 450 V/milshort term; ASTM D149
Dissipation Factor 0.00090
@Frequency 1e+6 Hz
ASTM D150
 0.0010
@Frequency 1000 Hz
ASTM D150
 0.0084
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 124 secASTM D495
Comparative Tracking Index 100 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 55.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 53.0 µm/m-°CISO 11359-2
Specific Heat Capacity 1.83 J/g-°C
Melting Point 280 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 400 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °CISO 75-1, -2
 220 °FASTM D648
Deflection Temperature at 8.0 MPa 95.0 °CISO 75-1, -2
Glass Transition Temp, Tg 90.0 °CISO 11357-1,-2,-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 295 - 330 °CISO 294
Mold Temperature 135 - 160 °CISO 294
Drying Temperature 110 - 120 °C
Dry Time 3.00 - 4.00 hour
Moisture Content <= 0.020 %
 
Descriptive Properties
Injection moldingYes
Sheet extrusion0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 205 PPS, Unfilled
Celanese FORTRON 320 PPS, Unfilled
Celanese FORTRON 214 PPS, Unfilled
Celanese FORTRON 309 PPS, Unfilled
Overview of materials for Polyphenylene Sulfide (PPS); Molded

PHCQ258 / 178713

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.