MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin NEOFLON® AF-0012 PFA Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: NEOFLON PFA film is a high performance film made from tetrafluoroethylene and perfluoroalkyl vinyl ether (PFA).

Information provided by Daikin Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.500 mil
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.040 - 0.060
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.92 - 2.12
@Frequency 1000 Hz
ASTM D150
 1.92 - 2.12
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.00010 - 0.00021
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
Oxygen Index >= 95 %
 
Descriptive Properties
Roll Length200 m
Roll Weight6 kg
Roll Width1150 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin NEOFLON® AF-1150 PFA Film
Daikin NEOFLON® AP-201 PFA
AGC Fluon® P-805UP PFA Perfluoropolymer
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded

PDAIK047 / 29339

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.