MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kazanorgsintez 107-30 KTU-2 Polyethylene Masterbatch, Carbon Black Filled
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Masterbatch Grade

Material Notes: Production Method: Made from LDPE of appropriate grades and low pressure polyethylene of low, medium, and high density with average concentration of carbon black 30% or 40% and required thermostabilizers for use in goods contacting food, drinking water, and for toy production.

Application: Grades are intended for production of HDPE and LDPE stabilized compositions.

Information Provided by Kazanorgsintez

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.20 %<= 0.20 %
Carbon Black Loading 30 - 43 %30 - 43 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ White 8750 Concentrate Based In HDPE
A. Schulman POLYBATCH™ Red 5505 Concentrate Based In Polyethylene
SPS Guang Zhou REMAK™ 7001RM4 Flame-retarded PS masterbatch
Multibase Multibatch® ME 50024 Anti-blocking Masterbatch
Meilian Chemical PE105B WHITE MASTERBATCH

PKAZAN030 / 127349

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.