MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Blow Molding Grade

Material Notes: Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength properties, along with excellent drawability, makes this a very versatile packaging film resin.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccExxonMobil Method
Thickness 1.00 mil
Melt Flow 1.0 g/10 minExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1300 psiat 2% offset; ASTM D882
Film Tensile Strength at Yield, TD 1400 psiat 2% offset; ASTM D882
Film Elongation at Break, MD 500 %ASTM D882
Film Elongation at Break, TD 700 %ASTM D882
Puncture Energy 3.17 ft-lbExxon Mobil Method
Elmendorf Tear Strength, MD 280 g/milASTM D1922
Elmendorf Tear Strength, TD 460 g/milASTM D1922
Dart Drop 560 g/milASTM D1709
Film Tensile Strength at Break, MD 11000 psiASTM D882
Film Tensile Strength at Break, TD 9100 psiASTM D882
1% Secant Modulus, MD 26600 psiASTM D882
1% Secant Modulus, TD 29700 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 246 °FPeak Melting Temperature; ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 18 %ASTM D1003
Gloss 42 %45°, MD; ASTM D2457
 42 %45°, TD; ASTM D2457
 
Descriptive Properties
FeaturesPPA and Thermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exceed™ 1018CA Metallocene Polyethylene Resin (European Grade)
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
Dow AFFINITY™ EG 8150G Ethylene alpha-olefin copolymer
Dow AFFINITY™ EG 8100G Ethylene-octene copolymer

PEXB116 / 37421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.