MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 2552 Damping Foil
Categories: Polymer; Tape

Material Notes: 3M™ Damping Foil 2552 consists of a room temperature pressure sensitive viscoelastic polymer on a dead soft aluminum foil and is designed for application to vibrating panels and support members. The combination of viscoelastic polymer and an aluminum foil backing (a constrained layer damper, CLD) has proved to be a unique construction with exceptional ability to control resonant vibrations in the temperature range of 0°to 60°C, with survivability from -32°C to 80°C.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 5.00 milAcrylic Viscoelastic Polymer
 10.0 milAluminum Backing
 15.0 milTotal
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 58.1 MPaASTM D3759
Elongation at Break 12 %ASTM D3759
Peel Strength 4.0625 pliAdhesion to Steel; ASTM D3330
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 60.0 °CPeak damping
 80.0 °C
Minimum Service Temperature, Air -32.0 °C
 0.000 °CPeak damping
 
Descriptive Properties
Liner58# poly-coated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 4014 Damping Aluminum Foam Sheet
SMAC SMACMOUNT® 1195S Damping Material
304 Stainless Steel
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, Viscoelastic
Asahi Kasei Xyron™ VT31Z PPE/PS, Acoustic Damping

PMM34452 / 169199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.