MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Hysol EA 9695 Film Adhesive
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Second generation, low flow, composite bonding film; excellent environmental resistance. Composite structure repair, cure and co-cure with composite laminates. Qualified to Airbus. Data from .050 psf, 250 g / m2.
    Applications:
  • Composite Bonding
  • Metal and Honeycomb Bonding
  • Composite Surfacing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 8.30 MPaFlatwise
Adhesive Bond Strength 19.3 MPa
@Temperature 132 °C
Composite double overlap shear
 30.3 MPa
@Temperature -55.0 °C
Composite double overlap shear
 34.5 MPa
@Temperature 25.0 °C
Composite double overlap shear
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air >= 149 °C
Glass Transition Temp, Tg 86.0 °Cwet, 121°C cure
 95.0 °Cwet, 175°C cure
 122 °Cdry, 121°C cure
 150 °Cdry, 175°C cure
 
Processing PropertiesOriginal ValueComments
Cure Time 1.50 hour
@Temperature 177 °C
 1.50 hour
@Temperature 121 °C
 
Descriptive Properties
Out-Time (days)90at 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Hysol EA 934NA Paste Adhesive System
Henkel Hysol EA 9686 Film Adhesive
Henkel Hysol EA 9696 Film Adhesive
Henkel Hysol EA 9321 Paste Adhesive System
Henkel Hysol EA 9320NA Paste Adhesive System

PHENK837 / 146842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.