MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecatron® XP-85 Compression Molded PPS Compound, with 30% Carbon Fiber
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler

Material Notes: Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.

TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.

Applications:

  • Fuel Injectors
  • Manifolds
  • Pumps
  • Pistons
  • Gears
  • V-Packing Gaskets
  • Bearings

Information provided by Ensinger Special Polymers, Inc.

Vendors: Ensinger Special Polymers, Inc. provides consistent, high quality compression molded stock shapes of engineering thermoplastics. Common shapes include rings, rods, plates, tubes, and discs. Large diameter rings up to 90" OD are available.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ASTM D792
Filler Content 30 %30 %
Water Absorption 0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9898ASTM D785
Hardness, Shore D 8787ASTM D2240
Tensile Strength 53.8 MPa7800 psiASTM D638
Elongation at Break 1.3 %1.3 %ASTM D638
Tensile Modulus 4.83 GPa700 ksiASTM D638
Flexural Strength 107 MPa15500 psiASTM D790
Flexural Modulus 10.3 GPa1500 ksiASTM D790
Flexural Strain at Break 1.1 %1.1 %ASTM D790
Compressive Strength 165 MPa24000 psi10% Deformation; ASTM D695
Compressive Modulus 5.24 GPa760 ksiASTM D695
Izod Impact, Notched 0.310 J/cm0.580 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.110.11ASTM D1894
Coefficient of Friction, Static 0.130.13ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 839 ohm-cm839 ohm-cmASTM D257
Surface Resistance <= 842 ohm<= 842 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 254 °C490 °FASTM D648
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber
Celanese Nilit FRIANYL B63 CV20 Nylon 6.6 for injection molding, 20% carbon fiber reinforced
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black
DuPont Mobility and Materials Vespel® SCP-50094 Polyimide
Ensinger Tecapeek® XP-114 Compression Molded PEEK Compound, 40% Carbon Fiber

PENSIN960 / 140833

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.