MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay HTM® 556 BMI
Categories: Polymer; Thermoset; Bismaleimide (BMI)

Material Notes: HTM 556 is a controlled flow, toughened bismaleimide (BMI) matrix system offering improved handling characteristics and after an appropriate post-cure, thermal cycling capability up to 250°C (482°F). HTM556 has been developed for structural applications where continuous service temperatures exceed 200°C (392°F)

Features & Benefits:

  • 30 days out life at 21°C (70°F)
  • 12 months storage at -18°C (0°F)
  • Controlled flow
  • Excellent tack and drape with improved ambient temperature tack stability
  • No hot debulks required
  • Free-standing post-cure
  • Maximum DMA E’ onset Tg of 270°C (518°F) after post-cure to 240°C (240°F)
  • Upper service temperature 250°C (482°F)
Note 1: Material: HTM556-T700G (12K)-145 g/m2-32%RW; Cure cycle: 6 hours at 190°C (374°F), 6.2 bar (90 psi); Post-cure: 6 hours at 240°C (464°F)
Note 2: Material: HTM556-HTS (12K)-145 g/m2-32%RW; Cure cycle: 6 hours at 190°C (374°F), 6.2 bar (90 psi); Post-cure: 6 hours at 240°C (464°F)
Note 3: Material: HTM556-IM7(6K)-plain weave-38%RW; Cure cycle: 6 hours at 190°C (374°F), 6.2 bar (90 psi); Post-cure: 6 hours at 255°C (437°F)
Note 4: 8 Material: HTM556-CF0800 (6K)-375 g/m2-2x2 twill; Cure cycle: 6 hours at 190°C (374°F), 6.2 bar (90 psi); Post-cure: 6 hours at 255°C (437°F)
Note 5: HTM556-CF0800 (6K)-375 g/m2-2x2 twill; Cure cycle: 6 hours at 190°C (374°F), 6.2 bar (90 psi); Post-cure: 6 hours at 240°C (464°F)
Note 6: HTM556-CF1218 (6K)-375 g/m2-2x2 twill T800; Cure cycle: 6 hours at 190°C (374°F), 6.2 bar (90 psi); Post-cure: 6 hours at 240°C (464°F)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.242 g/ccCured
Storage Temperature -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 114200 psi0°, Note 4; ASTM D3039
 145000 psi0°, Note 3; ASTM D3039
 326200 psi0°, Note 2; ASTM D3039
 367800 psi0°, Note 1; ASTM D3039
Tensile Modulus 62.5 GPa0°, Note 4; ASTM D3039
 65.0 GPa0°, Note 3; ASTM D3039
 144 GPa0°, Note 2; ASTM D3039
 151 GPa0°, Note 1; ASTM D3039
Flexural Strength 126500 psi0°, Note 4; ASTM D790
 282800 psi0°, Note 1; ASTM D790
 370000 psi0°, Note 2; ASTM D790
Flexural Modulus 20.3 GPa0°, Note 2; ASTM D790
 20.6 GPa0°, Note 1; ASTM D790
 49.5 GPa0°, Note 3; ASTM D790
Compressive Strength 90.0 MPa0°, Note 3; ASTM D6641
 727 MPa0°, Note 4; ASTM D6641
 788 MPa0°, Note 6; ASTM D6641
 1622 MPa0°, Note 1; ASTM D6641
 1800 MPa0°, Note 2; ASTM D6641
Compressive Modulus 59000 MPa0°, Note 4; ASTM D6641
 60000 MPa0°, Note 3; ASTM D6641
 115000 MPa0°, Note 2; ASTM D6641
 127000 MPa0°, Note 1; ASTM D6641
Shear Strength 6000 psi
@Thickness 6100 mm
0° Interlaminar, Note 5; ASTM D2344
 6300 psi
@Thickness 6100 mm
0° Interlaminar, Note 6; ASTM D2344
 7500 psi
@Thickness 5080 mm
0° Interlaminar, Note 5; ASTM D2344
 7900 psi
@Thickness 5080 mm
0° Interlaminar, Note 6; ASTM D2344
 8400 psi
@Thickness 4450 mm
0° Interlaminar, Note 5; ASTM D2344
 8700 psi
@Thickness 4450 mm
0° Interlaminar, Note 6; ASTM D2344
 9100 psi
@Thickness 610 mm
0° Interlaminar, Note 6; ASTM D2344
 10100 psi
@Thickness 5080 mm
0° Interlaminar, Note 1; ASTM D2344
 10100 psi
@Thickness 5080 mm
0° Interlaminar, Note 2; ASTM D2344
 10500 psi
@Thickness 610 mm
0° Interlaminar, Note 5; ASTM D2344
 11000 psi
@Thickness 610 mm
0° Interlaminar, Note 3; ASTM D2344
 11400 psi
@Thickness 610 mm
0° Interlaminar, Note 4; ASTM D2344
 16600 psi
@Thickness 610 mm
0° Interlaminar, Note 1; ASTM D2344
 18400 psi
@Thickness 610 mm
0° Interlaminar, Note 2; ASTM D2344
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °C
Glass Transition Temp, Tg 190 °CDMA E' onset, 6 hrs at 190°C, 90 psi
 260 °CDMA E' onset, 6 hrs at 190°C, 90 psi + 6 hrs at 225°C
 270 °CDMA E' onset, 6 hrs at 190°C, 90 psi + 6 hrs at 240°C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay HTM® 552 Bismaleimide Resin
HOS-Technik Homide 250 Bismaleimide Resin
Hexcel® HexPly® F650 Bismaleimide Resin
Solvay FM® 6604-1 BMI Foaming Adhesive
Solvay CYCOM® 5250-4 BMI Prepreg Neat Resin

PCYTED137 / 180439

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.