MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Wacker® AF 23 Silicone Softener Fluid
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: A general purpose, high molecular weight reactive aminoethylaminopropyl fluid. Imparts a very soft hand with normal yellowing characteristics associated with amino silicones.

Application: WACKER® AF 23 is particularly suitable as an active substance in softener formulations for the impregnation of fibers and textiles. WACKER® AF 23 imparts a very soft, drapable, and elastic handle to woven and knitted fabrics. WACKER® AF 23 is considered to be the best softening agent for cotton woven and knit fabrics made of cotton or cotton/PES blends. WACKER® AF 23 improves the wash-and-wear properties and the crease recovery angle, sewability and tear strength and reduces abrasion loss. The effects are fast to washing and dry cleaning. WACKER® AF 23 has very little effect on the degree of white in a softener formulation when usual application conditions are adhered to. As a rule, no adverse effect on the shade or color fastness properties of colored goods is observed. As part of formulations used as fill fiber finish WACKER® AF 23 imparts excellent slickness and resilience to the fiber.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 5.0 %<= 5.0 %
Viscosity 3000 - 6000 cP3000 - 6000 cP
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Amine number0.3
AppearanceClear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Wacker® AF 21 Functional Silicone Fluid
Wacker Pulpsil® 235 C Silicone Antifoam Compound
Wacker Pulpsil® 160 C Silicone Antifoam Compound
Wacker Powersoft® FE 55 Silicone Softener
Wacker Powersoft® AE 66 Silicone Softener

PWACK9694 / 205223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.