MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Equate EGDA-6888 HDPE Film Extrusion Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: EGDA-6888 is a high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density have been optimized to give excellent bubble stability at high extrusion rates with high film strength and rigidity. The combination of high strength and excellent drawdown-ability makes EGDA-6888 ideal for down gauging in many applications.

Applications: Tubular films produced from EGDA-6888 are recommended for high strength grocery sacks, shopping bags, produce bags and high quality thin films for multiwall sack liners and replacements for thin paper products. Films are nearly gel-free and have excellent treatability. They are suited for printing of high quality graphics.

Information provided by Equate

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.560 g/ccASTM D1895
Density 0.952 g/ccASTM D792
Thickness 15.0 micronsAs Tested
High Load Melt Index 10 g/10 min
@Load 21.6 kg
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 380 %
@Thickness 0.0150 mm
ASTM D882
Film Elongation at Break, TD 550 %
@Thickness 0.0150 mm
ASTM D882
Elmendorf Tear Strength, MD 70.0 g/micron
@Thickness 0.0150 mm
ASTM D1922
Elmendorf Tear Strength, TD 150 g/micron
@Thickness 0.0150 mm
ASTM D1922
Dart Drop 11.3 g/micron
@Thickness 0.0150 mm
ASTM D1709 A
Dart Drop Test 170 gF50; ASTM D1709 A
Film Tensile Strength at Break, MD 60.0 MPa
@Thickness 0.0150 mm
ASTM D882
Film Tensile Strength at Break, TD 57.0 MPa
@Thickness 0.0150 mm
ASTM D882
1% Secant Modulus, MD 1220 MPa
@Thickness 0.0150 mm
ASTM D882
1% Secant Modulus, TD 1470 MPa
@Thickness 0.0150 mm
ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 131 °CEquate Test Method
 
Processing PropertiesOriginal ValueComments
Blow-up Ratio (BUR) 4.04:1 As Tested

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Equate EFDC-7087 LLDPE Film Extrusion Resin
Equate EFDC-7050 LLDPE Film Extrusion Resin
Equate EFDA-7047 LLDPE Film Extrusion Resin
Equate EMDA-6200 HDPE Blow Molding Resin
Equate EMDA-8920 HDPE Injection Molding Resin

PEQUAT903 / 150431

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.