MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating parts.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.800 g/cc
Density 1.32 g/ccISO 1183
Moisture Absorption at Equilibrium 2.1 - 2.5 %23°C; 50% RH; ISO 62
 2.3 %50% RH
 7.1 %Saturation
Water Absorption at Saturation 6.8 - 7.4 %ISO 62
Viscosity Measurement 140ISO 307
Linear Mold Shrinkage 0.0035 cm/cmrestricted
Melt Flow 72.6 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 30.0 MPa
@Strain 1 %,
Temperature 150 °C
ISO 527
 35.0 MPa
@Strain 1 %,
Temperature 120 °C
ISO 527
 38.0 MPa
@Strain 1 %,
Temperature 100 °C
ISO 527
 45.0 MPa
@Strain 2 %,
Temperature 150 °C
ISO 527
 60.0 MPa
@Strain 2 %,
Temperature 120 °C
ISO 527
 65.0 MPa
@Strain 2 %,
Temperature 100 °C
ISO 527
 70.0 MPa
@Strain 1 %,
Temperature 60.0 °C
ISO 527
 83.0 MPa
@Strain 1 %,
Temperature 23.0 °C
ISO 527
 100 MPa
@Strain 1 %,
Temperature -20.0 °C
ISO 527
 100 MPa
@Strain 2 %,
Temperature 60.0 °C
ISO 527
 143 MPa
@Strain 2 %,
Temperature 23.0 °C
ISO 527
 170 MPa
@Strain 2 %,
Temperature -20.0 °C
ISO 527
Tensile Strength, Yield 160 MPa50 mm/min; ISO 527-1/-2
Elongation at Yield 3.5 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 8.00 GPaISO 527-1/-2
Flexural Strength 220 MPaat max force; ISO 178
Flexural Modulus 7400 MPaISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 75.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.025
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 450 VTest solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 - 25.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 11359-1/-2
CTE, linear, Transverse to Flow 60.0 - 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 11359-1/-2
Specific Heat Capacity 1.50 J/g-°C
Thermal Conductivity 0.350 W/m-KDIN 52612
Melting Point 220 °CDIN 53765
Maximum Service Temperature, Air 145 °Cfor 50% loss of tensile strength after 20000hr
 175 °Cfor 50% loss of tensile strength after 5000hr
 200 °C
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-1/-2
Decomposition Temperature >= 300 °C
UL RTI, Electrical 130 °C
@Thickness 1.50 mm
746B
UL RTI, Mechanical with Impact 95.0 °C
@Thickness 1.50 mm
764B
UL RTI, Mechanical without Impact 130 °C
@Thickness 1.50 mm
764B
Flammability, UL94 HB
@Thickness 1.60 mm
Ignition Temperature >= 400 °CASTM D129
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CHopper Throat
Zone 1 260 °CFeed Zone
Zone 2 270 °CCompression
Zone 3 280 °CMetering-zone
Zone 4 280 °CNozzle
Melt Temperature 270 - 290 °CInjection-molding/Extrusion
 280 °COptimal
Mold Temperature 80.0 °COptimal
 80.0 - 90.0 °CInjection-molding
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.030 - 0.060 %Optimal
 <= 0.15 %
 
Descriptive Properties
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned)
BASF Capron® GR30 30% Glass-Filled Nylon 6 (Dry)
BASF Ultramid® B3WG5 BK 00654 PA6 25% Glass Filled BK (Dry)
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry)
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Dry, 20% Glass Filled

PBASG0264 / 131897

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.