MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form.

INNOPOL® CS 3-9120 SR5 is developed for producing injection molded automotive components.

Information provided by INNO-COMP

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
nozzle diam 2.095 mm; ISO 1133
Storage Temperature <= 60.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 25.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Yield 3.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2100 MPa1 mm/min; ISO 527-1,-2
Flexural Modulus 2200 MPaISO 178
Charpy Impact, Notched 2.20 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 4.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 108 °CISO 75-1,-2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 - 240 °CInjection
Middle Barrel Temperature 190 - 240 °CInjection
Front Barrel Temperature 190 - 240 °CInjection
Melt Temperature 210 - 250 °CInjection
Mold Temperature 10.0 - 50.0 °C
Moisture Content <= 0.070 %
 
Descriptive Properties
Resin DesignationPP-H/PP-B TD 17ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow INFUSE™ 9817 Olefin Block Copolymer
Dow INFUSE™ 9807 Olefin Block Copolymer
Dow INFUSE™ 9507 Olefin Block Copolymer
Dow INFUSE™ 9107 Olefin Block Copolymer
Dow INFUSE™ 9007 Olefin Block Copolymer

PINNO909 / 150109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.