MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled

Material Notes: Ultramid A 3HG2 is a 10% glass fiber reinforced grade of nylon 6/6 for injection molding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Water Absorption 7.0 %ISO 62
Moisture Absorption at Equilibrium 2.1 %23°C/50% R.H.; ISO 62
Viscosity Number 148 cm³/g
Linear Mold Shrinkage 0.0080 cm/cmASTM Data; MD
Melt Flow 80 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPa0.2 in/min; ASTM Test
Tensile Strength, Ultimate 100 MPa5mm/min; ISO 527
Elongation at Break 3.0 %5mm/min; ISO 527
 3.0 %0.2 in/min; ASTM Test
Tensile Modulus 4600 MPa1mm/min; ISO 527
 4620 MPaASTM Test
Flexural Modulus 4480 MPaISO Data
 4480 MPaASTM Test
Izod Impact, Notched 0.530 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Notched (ISO) 5.50 kJ/m²ISO Test
Charpy Impact Unnotched 3.00 J/cm²ISO 179
Charpy Impact, Notched 0.700 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 33.0 µm/m-°CISO 11359
CTE, linear, Transverse to Flow 75.0 µm/m-°CISO 11359
Melting Point 260 °C10 K/min
 260 °CASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 210 °CASTM Test
 210 °CISO 75
Vicat Softening Point 250 °C(50 °C/h / 50N) - B/50; ISO 306
Flammability, UL94 HB
@Thickness 1.65 mm
 HB
@Thickness 0.800 mm
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry)
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)
BASF Ultramid® A3HG5 BK00564 25% Glass Filled PA66 (Dry)

PBASF9229 / 84993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.