MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Premi-Glas® 1266 (Injection Compression Molded) Glass Reinforced TMC
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Description: Premi-Glas® 1266 is a glass reinforced thermoset molding compound designed for automotive under the hood applications.

Key features and benefits:

  • Designed for Injection or Injection/Compression Molding
  • Excellent resistance to automotive chemicals and fluids, and to salt spray
  • Replaces Cast Metals for Reduced Noise, Vibration and Harshness
  • TMC compounding process preserves glass integrity for excellent strength vs. BMC
  • Excellent thermal properties and elevated temperature modulus retention
  • Mechanical data below are from injection-compression panels; see separate data sheet for compression molded properties as per some specification requirements

Market: Composite PowerTrain

Information provided by Premix.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.74 g/cc
Water Absorption 0.20 %ISO 62
Linear Mold Shrinkage 0.00065 cm/cmPolymerization Shrinkage
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 40.0 MPaISO 527
Tensile Modulus 12.0 GPaISO 527
Flexural Strength 80.0 MPaISO 178
Flexural Modulus 10.0 GPaTangent; ISO 178
Poissons Ratio 0.27
Shear Modulus 4.70 GPaCalculated
Izod Impact, Unnotched (ISO) 10.0 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°CZ Direction
CTE, linear, Transverse to Flow 25.0 µm/m-°CXY Direction
Thermal Conductivity 0.400 W/m-K
Deflection Temperature at 1.8 MPa (264 psi) >= 270 °CISO 75
Glass Transition Temp, Tg 204 °CASTM D4065-01
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 °CInjection or Injection-Compression Molding
Clamp Pressure <= 1000 psiMolding Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 1265 VE 1265-VE (Injection Compression Molded) Glass Reinforced Vinyl Ester TMC
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI)
Mitsubishi Chemical Advanced Materials Duratron™ T4540 PAI Polyamide-imide, compression molded
Overview of materials for Epoxy Molding Compound
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled

PPREMI07 / 58134

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.