MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Supreme SAE 10W-30 Motor Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Supreme Motor Oils are premium quality automotive engine oils.

Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhibitor, and foam suppressant additives.

The high viscosity index of Chevron Supreme Motor Oils ensures low viscosities at low temperatures for easy cold starting and rapid warm-up and high viscosities at high temperatures for fuel economy, oil economy, and effective protective films for engine parts.

Their antiwear additive provide excellent wear protection of critical engine parts.

A high level of dispersancy in Chevron Supreme Motor Oils protects against deposit and sludge formation in stop-and-go driving and sustained high temperature operation, and protects against corrosion.

Their excellent high temperature oxidation stability prevents viscosity increase and oil gelling in the crankcase. They keep PCV systems clean to maintain smooth engine performance.

Applications

Chevron Supreme Motor Oils are recommended for all four-stroke gasoline engines used in passenger cars, light trucks, power boats, motorcycles, and other mobile and stationary equipment. They are excellent for high revving engines in small cars and light trucks. All grades are specially formulated for using in turbocharged engines.

SAE 10W-30 is recommended for many older vehicles and a few late model cars and trucks, often those with larger 6-cylinder and V-8 and/or high performance engines. SAE 10W-30 provides improved fuel economy relative to heavier viscosity grades.

Key Words: CPS Number: 220019; MSDS Number: 6717
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 30.4 °
Viscosity 5800 cP
@Temperature -25.0 °C
Cold Crank
Viscosity Measurement 135Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 73.5 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 10.8 cStASTM D445
Ash 0.90 %Sulfated Ash wt%
 
Chemical PropertiesOriginal ValueComments
Total Base Number 7.4ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -35.0 °CASTM D97
Flash Point 232 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.094 %
Zinc, Zn 0.103 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Havoline® SAE 10W-30 Synthetic Motor Oil
Ethylene glycol, C2H6O2
Water, H2O
ExxonMobil Mobil 1 10W-30
Special Metals INCONEL® Alloy 600

WCHEV027 / 74642

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.