MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mid-Mountain Materials SILTEX® 1800 Amorphous Silica Industrial Textile
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide

Material Notes: SILTEX® 1800 is a family of high performance textiles comprised of high purity, high strength amorphous silica fibers. SILTEX® 1800 Industrial Textiles demonstrate excellent thermal stability, have insulating values up to 1800ºF (980ºC), and are designed for use where severe temperature conditions exist.

Information provided by Mid-Mountain Materials

Key Words: MIL-I-24244
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 1260 °C2300 °F
Maximum Service Temperature, Air 982 °C1800 °FContinuous
 1260 °C2300 °FShort term
 
Component Elements PropertiesMetricEnglishComments
SiO2 96 %96 %
 
Descriptive Properties
Abrasion ResistancePoor
Acid ResistanceGood
Alkali ResistancePoor
CertificationMIL-I-24244May be manufactured for conformance
ColorWhite or Tan
Solvent ResistanceExcellent
Sunlight and Aging ResistanceExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mid-Mountain Materials SILTEX® 18 Amorphous Silica Textile
Fiberglass Grade B
E-Glass Fiber, Generic
D-Glass Fiber, Generic
C-Glass Fiber, Generic

CMID07b / 141226

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.