MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PolyMirae Clyrell EC340Q Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Clyrell EC340Q is a specially designed nucleated polypropylene copolymer for injection molding. Clyrell EC340Q offers an excellent impact / stiffness balance, easy processing, low stress whitening with very high gloss and low shrinkage for use in toys, sport, leisure, food packaging, containers, housewares, consumer goods and similar applications. The unique low shrinkage of Clyrell EC340Q suggests its potential use also in applications which are typically dominated by styrenics. This grade is suitable for food contact.

Product Features: High gloss/ low stress whitening/ low shrinkage/ excellent impact at low temperature

Typical Applications: Injection molding for toys, food packaging, containers, housewares, consumer goods/ Compounding use

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 220 kg(f)/cm²ASTM D638
Flexural Modulus 10000 kg(f)/cm²ASTM D790
Izod Impact, Notched 6.00 kg-cm/cm
@Temperature -20.0 °C
ASTM D256
 50.0 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 110 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Moplen RP343N Injection Molding Grade Polypropylene
PolyMirae Clyrell EC340R Injection Molding Grade Polypropylene
PolyMirae Moplen EP500M Injection Molding Grade Polypropylene
PolyMirae Moplen EP5015 Injection Molding Grade Polypropylene
PolyMirae Moplen RP340N Injection Molding Grade Polypropylene

PMIRAF09 / 183230

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.